November 25, 2026

Divinyl ether YLD-S0101 is a diethylene glycol divinyl ether, CAS 764-99-8, that cures by cationic polymerization, not by amine addition. The product page states purity min. 99.0 %, APHA max. 50 and water max. 0.5 %; the companion grade YLD-S0102, CAS 765-12-8, is the triethylene glycol homologue.

How a Divinyl Ether Differs from a Glycidyl Ether

A glycidyl ether carries an epoxide ring that opens by nucleophilic addition, so its dosage follows AHEW and EEW. A divinyl ether carries an electron-rich double bond that polymerizes under a cation, typically a sulfonium salt activated by ultraviolet light.

The two react by different routes and are not interchangeable in a stoichiometric calculation. No phr figure can therefore be derived from 100 × AHEW ÷ EEW. A vinyl ether diluent is dosed by initiator level and viscosity target instead.

Published Specification of YLD-S0101 and YLD-S0102

Table 1. Values as published on the two product pages. The boiling point row carries no pressure reference on the page, so it should not be read as an atmospheric figure.

Item YLD-S0101 YLD-S0102
Chemical name Diethylene glycol divinyl ether Triethylene glycol divinyl ether
CAS No. 764-99-8 765-12-8
Appearance Colorless transparent liquid Colorless or light yellow liquid
Assay, % Purity min. 99.0 DVE-3 content min. 98.0
Color, APHA max. 50 not stated
Water, % max. 0.5 max. 0.20
Density, g/mL at 25 °C not stated 0.99
Boiling point, °C not stated 120–126

From the molecular formulas, the vinyl equivalent weight calculates to 79.1 g per vinyl group for C8H14O3 at 158.19 g/mol, against 101.1 g/eq for C10H18O4 at 202.25 g/mol. Both figures are calculated, not measured, and should be confirmed against our TDS.

Dosage of a Divinyl Ether Diluent in phr

A divinyl ether enters a UV-cationic coating as the reactive fraction, typically 10–30 phr against an epoxy or oxetane base, with a triarylsulfonium photoinitiator at 1–3 phr. Neither product page publishes a recommended loading, so these are application ranges.

Table 2. Starting points for a formulation trial, separated by basis; only the equivalent weights are derived from published data.

Parameter Starting range Basis
Vinyl ether fraction 10–30 phr application range, not published
Photoinitiator 1–3 phr application range, not published
Vinyl equivalent weight, YLD-S0101 79.1 g/eq calculated from C8H14O3
Vinyl equivalent weight, YLD-S0102 101.1 g/eq calculated from C10H18O4

Grade Selection and Next Step

YLD-S0101 carries the higher vinyl density at 79.1 g/eq and is the faster of the pair. YLD-S0102 states DVE-3 content min. 98.0 % and density 0.99 g/mL at 25 °C, and its longer glycol chain gives the more flexible network.

Neither page publishes viscosity, so a dilution level should be fixed against the TDS rather than against a catalogue figure. For a first trial, request 500 g of YLD-S0101 and run it against the same loading of YLD-S0102 in the intended coating. Compare gel time at equal photoinitiator level, then check adhesion once the film has cured. The coatings application note sets out the film requirements the pair has to meet.